Raw mix for the production of portland cement clinker
In the production of clinker from this mix, the temperature at which the clinker formation process was completed was lowered from 1500#176; C. to 1420#176; C. The strength of clinker produced using this raw mix was 550 kgf/cm 2. EXAMPLE 2. A raw mix for the production of portland cement clinker of the following composition (% by weight) was prepared: